5000 PSI compressive creep test at 200 degrees C after 4870 hours (approx. 6 mo.) showing one fixture disassembled. Prior to disassembly, heavy m.l. wire to wire failed at 2800 and 350V AC while 3-one mil layers of caption withstood 5000V AC without breakdown from wire to iron. Note: Copper wire deformedium
Title: 5000 PSI compressive creep test at 200 degrees C after 4870 hours (approx. 6 mo.) showing one fixture disassembled. Prior to disassembly, heavy m.l. wire to wire failed at 2800 and 350V AC while 3-one mil layers of caption withstood 5000V AC without breakdown from wire to iron. Note: Copper wire deformedium
Creator: General Electric Company
Date Created: 1965-10-11
Physical Dimensions: 8 x 10
Original Language: English
Subject Keywords: Testing; General Electric Company.;
Rights: This digital image may be used for educational uses. Please cite as miSci- Museum of Innovation & Science. Prior written permission is required for any other use of the images from miSci.
Get the app
Explore museums and play with Art Transfer, Pocket Galleries, Art Selfie, and more